QuLPA-Fe10Cr

Product information "QuLPA-Fe10Cr"

The material is preferred for changes to and repairs of cavities subjected to high stress of the tempered materials: 1.2311, 1.2312, 1.2162 , 1.2738, 1.2764 and 1.2767.
Achievable hardness of approx. 27 - 38 HRC. Depending upon the working
Packaging: 4 x 5 kg bottles

Material analysis
C: 0,1 | Si: 0,6 | Mo: 0,5 | Mn: 1,0 | Cr: 1,2 | Fe: Rest
Achievable hardness: 27 - 38 HRC
Grain size: 45 - 90 µm
Recommendations for basis material: 1.2162, 1.2311, 1.2312, 1.2738, 1.2764, 1.2767, 13CrMo 4 4, 25CrMo4, 42CrMo4, AIS4130, AISI4140, GS-17 CrMo5 5
Refinish: Hardenable , chrome-plated , erodible , etable , nitridable , polishable, remunerable , structurable
Wire: Powder